The material investigated was a 316LVM austenitic stainless steel. The grain refinement was achieved by hydrostatic extrusion (HE) at room and elevated (900oC) temperature. The samples were nitrided in low-temperature plasma assisted nitriding process. The nitriding process results in the formation of nitride layer, whose thickness was to some extent influenced by the substrate grain structure. The sample HE processed at room temperature with a true strain of 2.3 features an uniformly refined microstructure consisting of nanotwins and shear bands on the cross section and a fiber-like microstructure on the longitudinal section. The sample HE processed at elevated temperature exhibits the microstructure with equiaxial subgrains. The results are discussed in terms of the role different types of grain boundaries as fast diffusion paths as well as trapping sites for diffusing nitrogen atoms. The properties such as corrosion and wear resistance were also evaluated and attributed to specific features of the nitride layers.
The mechanical properties of steels are strongly affected by grain size and chemical composition variations. Many industrial developments have been carried out both from the point of view of composition variation and grain size in order to exploit the effect of these variables to improve the mechanical proprieties of steels. It is also evident that recrystallization and grain growth are relevant to the mechanical properties of steels, thus suggesting the necessity of mathematical models able to predict the microstructural evolution after thermo-mechanical cycles. It is therefore of primary importance to study microstructural changes, such as grain size variations of steels during isothermal treatments through the application of a mathematical model, able in general to describe the primary recrystallization and grain growth in metals. This paper deals with the recrystallization and grain growth modelling of steels and takes into account the effect of recrystallization and Zener drag effect. A general continuity equation is proposed describing in continuous way recrystallization and grain growth phenomena without taking into account textures effect. The effect of input parameters is analyzed.
Magnetic and transport properties of cold rolled SUS304 stainless steels were investigated via measurements of X-ray diffraction, magnetization, thermoelectric power (TEP), thermal conductivity and electrical resistivity at low temperatures below 300 K. The X-ray diffraction spectra measured at room temperature indicated that the crystal structure of austenite phase transferred to that of martensite phase by a cold rolling. The volume fractions of the martensite phase to the austenite were evaluated using the diffraction peaks. Saturation magnetizations at 300 K were 1.6, 37.5, 72.6 and 105.6 emu/g for the reduction ratios of 0, 33, 50 and 75%, respectively. The TEP values at 300 K were found to be -1.3, -0.4, 1.6 and 2.9 micro V/K for the reduction ratios of 0, 33, 50 and 75%, respectively. The temperature variations of TEP of SUS304 and SUS316L in the austenite phase resemble each other, whereas TEP variations of martensite SUS304 is similar to that of SUS630. The present results of the volume fraction of martensite phase, magnetization and thermoelectric power reveal that there are linear relationships among these properties around room temperature. The least-square fit of the experimental data predicts a saturation magnetization of 141 emu/g and thermoelectric power of 4.3 micro V/K for SUS304 in the martensite phase at 300 K.
In this study, stainless steel corrosion resistant surface layer was prepared on carbon steel matrix by Twin-Wire Indirect Arc Welding (TWIAW). The arc stiffness increased with the increasing of the welding current and the amount of the CO2 in Ar+CO2 protective gas. The droplets formed by melting of positive and negative welding wires repelled each other, and the included angle between the two stand droplets decreased with the increasing of the welding current. Well appearance of stainless steel weld can be obtained on the surface of carbon steel matrix when the arc voltage was about 31V and the welding current was from 130A to 150A. The phase composition of the surfacing layer was austenite with a small amount of ferrite, which depends on the welding parameters and the angle between the two wire, besides, the highest content of ferrite was no more than 10%. With the increasing of welding current, the pitting potential of the composite layer decreases, resulting in the decreasing of the pitting corrosion resistance. However, only slight intergranular corrosion took place in the surfacing layer because of no sensitization or slight sensitization occurring, which was attributed to the low heat input in the TWIAW.
The corrosion resistance was studied electrochemically for an iron-based brazing filler metal F300 and a Ni-based brazing filler metal Ni613. Both austenitic stainless steel SUS316 and ferritic stainless steel SUS444 were used as base metals for these brazing filling metals. F300 showed a higher corrosion rate than those of Ni613 and both base metals and was less corrosion-resistive. While Ni613 showed a stronger depression effect of an anodic reaction than those of base metals, F300 showed little depression effect of the reaction. As an Fe-Ni phase dissolved preferentially in F300 and a finite laminated corrosive morphology was observed, the corrosion progression along a depth direction was suggested. These corrosion behavior depend on the difference of chemical composition of these brazing filler metals.
The change in the microstructure of weldment in HAZ depends on compositions, peak temperature and cooling rate. In the welds between carbon steel and austenitic stainless steel, the phase formation and carbides precipitation in HAZ are different on each side of the weld. Continuous cooling transformation diagrams (CCT), peak temperature profiles and cooling rates can be used to predict the change in the microstructure of the HAZ during the welding process. Optical microscopy, X – ray, TEM, EDS were used to determine the phases which formed in HAZ of carbon steel and austenitic stainless steel. The results of this study indicate that grain size in HAZ depended on the temperature at that point could be reached during the welding. Fully Martensitic layer observed at the interface in carbon side due to the combination of the rapid cooling subsequent to weld and local chemical composition. Cooling rate played the rule on forming Widmanstatten ferrite, upper Bainite and Pearlite. On the other hand, microstructure and grain size in HAZ of austenitic stainless steel were not affected by temperature and cooling rate. Carbides precipitation (M23C6, M7C3), however, were found in the boundary of grains.