Tin dioxide-zinc oxide (SnO2-ZnO) nanocomposites have been prepared at different contents of SnO2 concentration to ZnO by sol gel technique in presence of polyethylene glycol. The prepared samples were dried and annealed at 600 oC. Effect of SnO2:ZnO molar ratios (1.0:1.0, 0.5:1.0, 0.3:1.0, and 0.1:1.0, respectively) on the crystal structure, optical and photocatalytic properties have been investigated. The synthesized samples are characterized by X-ray diffraction, transmission electron microscopy, scanning electron microscopy, Raman spectroscopy, Fourier transform infrared spectroscopy, and N2 physical adsorption, Uv-Vis spectroscopy and photoluminescence measurements. The optical band gaps of SnO2-ZnO nanocomposites were obtained from UV-diffuse reflectance spectroscopy studies. The findings revealed that the photocatalytic activities of SnO2- ZnO nanocomposites were increased with decreasing of SnO2 content to ZnO. This result indicated that molar ratio showed the highest photocatalytic activity for the methylene blue photodegradation because of the enhanced charge separation derived from the coupling of ZnO with SnO2 due to the potential energy differences between SnO2 and ZnO.
A thermoelectric module produces an electromotive force utilizing a temperature difference between the substrates, which absorbs or generates heat. The issue of heat dissipation performance is important. In thermoelectric power generation, the substrate can be damaged unless the heat at high temperatures, which generates electrical energy due to the temperature difference, is released quickly. Therefore, for the thermoelectric module to be practical, a substrate with high heat dissipation properties should be applied. Currently, ceramic substrates (such as alumina, commonly used for these purposes) lack the sufficient heat dissipation performance; Therefore, substrates with high thermal conductivities have been studied recently for this purpose [1]. Since the thermal conductivity of alumina is low at 30 W/m·K, this study aims to study the fabrication of a plate for thermoelectric modules using Al, which has a thermal conductivity of 237 W/m·K. So, to produce a plate on which a copper circuit was formed, electrolytic etching, hydration processing, anodic oxidation, and copper electroplating were applied to aluminum. An oxide film serving as an insulating layer was formed on aluminum through anodic oxidation treatment, and platinum was coated by sputtering to produce conductivity. Finally, copper electroplating was performed on a substrate directly. In this structure, a copper plating layer on the insulating layer can serve as a conductive layer of circuit. Adhesion of the copper plating layer was also improved by electrolytic etching. As a result, the thermoelectric module fabricated in this study showed excellent adhesion and good insulation characteristics. It is expected that our findings can improve the life and performance of thermoelectric modules with high dissipation performance.
Dissimilar material joining is generally more challenging than that of similar materials, due to various factors such as the differences in chemical compositions and the physical and mechanical properties of the base metals welded
In this study, the metallurgical characteristics, and mechanical properties of dissimilar metals welds between duplex stainless and Low alloy steel have been evaluated. Duplex E2209 and Austenitic E309L filler metals were used to join this combination using multipass gas tungsten arc welding process.
The microstructure investigation was conducted with optical microscope, scanning electron microscope, Energy dispersive scanning and X-ray diffraction.
A higher value of hardness is recorded in a narrow zone between the fusion boundary and type II boundary, which is attributed to the presence of harder phases in this region, due to the migration of carbon from the HSLA side to the weld metal. Both of welds gave acceptable values of tensile strength and impact toughness.
Potentiodynamic polarization tests of different regions of the weld joints evaluated in 3.5% M NaCl solution show that E309 weld metal exhibit a higher corrosion resistance than E2209 weld metal.
This study is aimed at the investigation of the magnetic properties in the non-oriented electrical steels with 3.5% silicium. Conventional rolling at ambient temperature and progressive rolling at cryogenic temperature were used to obtain different strain-temperature conditions. Considering cryogenic conditions, total deformation was ε = 35%. Subsequently, the samples were annealed at temperatures T=<900; 1000; 1100> ° C. Measuring of the magnetic properties was carried out in an alternating magnetic field in frequencies f=< 50; 100; 150>Hz. In a frequency of 50 Hz, there were achieved smallest magnetic losses and therefore further measurements were made in a given frequency. Followed measurements of the magnetic induction were conducted at different intensities of the magnetic field. EBSD analyses were performed to obtain the IPF maps on which the resulting structure was evaluated after processing of the material. The specific magnetic losses were compared to different processing methods. The suitable condition is cryo-rolling followed by annealing at 900 ° C, for which the smallest magnetic losses was measured.
The comparison of conventional cold-rolling and progressive cryorolling processing is presented in this work. For cryogenic rolling condition the liquid nitrogen bath is used. Low temperature during rolling process prevent dynamic recovery of material what cause high dislocation density and increasing of stored energy. Therefore other deformation mechanisms are stared. While at ambient temperature, the main mechanism is slip, during deformation at cryogenic temperature the deformation bands and twinnig is present. All these factors have significat influence on resulting mechanical properties. In this work, the austenitic stainless steel and non-oriented electrical steel after conventional cold-rolling and cryogenic rolling after different total deformation were observed. The mechanical properties were tested by static tensile test at room temperature.
The aim of this work is to investigate cold worked Ti-6Al-4V alloy. The MAUD software (Materials Analysis Using Diffraction) was used to analyze the microstructural parameters evolution (crystallite size, root mean square strain (r m s) and dislocations density (ρ). The microstructural parameters of Ti-6Al-4V alloy exhibit typical values of cold deformation state. The results show a reduction in the crystallite size (coherent diffraction domains) as a function of the deformation. An increase in the microstrain and dislocations density with a factor of 10 after 85 % thickness reduction was obtained.
A new way of strengthening surface layers of sheet high-strength titanium alloys was tested experimentally. Sheet two-phase titanium alloy VT23 was selected as an object of research. It is shown that by impulse introduction of energy into the alloy and the use of colloidal solutions of hard alloys, one can not only significantly increase the initial plastic deformation of the alloy at a time, but also strengthen surface layers of the alloy by tens of percents.
One of today’s advanced heat treatment routes for high-strength steels is the Q&P process which delivers high ultimate strengths combined with good ductility. The resulting microstructure is a combination of martensite and small fractions of bainite and retained austenite. Retained austenite has the form of thin needles adjacent to martensite laths. The use of this process in industrial practice is complicated by the need for holding at the partitioning temperature when retained austenite becomes stabilized by carbon migration from super-saturated martensite. Engineers therefore seek process routes in which interrupting the cooling process at a particular temperature and holding at that temperature do not pose technological problems.
One of the available options is press hardening, often incorporated in the treatment of car body parts. 42SiCr steel, which is alloyed with manganese, silicon and chromium, was Q&P-processed using experimental sequences with various quenching and partitioning temperatures. The soaking time and temperature and cooling rates were identical to the parameters used in real-world processes. Correctly-chosen parameters led to martensitic-bainitic microstructures with a portion of retained austenite, ultimate strength of around 2000 MPa and A20 elongation of more than 10%.
Selection of appropriate quenchant could be determined the success or failure of a quenching process. The numerical simulation research of the quenching process for 100Cr6 steel specimen in different media, including water, oil, and Polyvinyl pyrrolidone (PVP) aqueous solutions was investigated in the present study. The results showed that the cooling mechanism in PVP solution quenchants was more effectively than water and oil quenchants. The distortion and crack of the quenching specimens were reduced in compared to water quenching medium. The mechanical properties which were not achievable by oil quenchant have resulted in the using polymer-based quenching medium.
Positron Lifetime Annihilation Spectroscopy (PALS) has been used to characterize friction stir weldments between 2017A-T4 and 7075-T6 commercial aluminum alloys. The PALS method is particularly sensitive to structural defects that can trap positrons. The welds were produced in two configurations: one with 2017A situated on the advancing side and 7075 on the retreating side and the other with the alloy positions reversed. The PALS measurements were performed on weld cross-sections at room temperature with a time resolution of 0.28 ns. The experimental spectra, each one consisting of approximately one million counts, were collected by a conventional fast-fast spectrometer and further analyzed by the LT software. Numerical analysis of PAL spectra showed that the best fit (values of χ2 close to unity) was obtained under the assumption that one sample component corresponds to the average positron lifetime.
The average positron lifetime vs. the distance from the weld center was recorded for both alloy configurations. It is believed that positron lifetimes primarily depended on the total area of planar defects, i.e. grain, subgrain and especially interphase boundaries. The 7075 base alloy contains a significant number of second phase particles since it is in T6 temper while the 2017A alloy, being in T4 temper, contains notably fewer second phase particles. Hence, a substantial difference in positron lifetimes exists between these base alloys. The positron lifetime curves also reflect the changes in sample substructures (examined by transmission electron microscopy) and the behavior in microhardness.
Severe plastic deformation (SPD) processes attracted attention in recent years as a method of grain refinement. SPD processes, such as equal channel angular pressing (ECAP), accumulative roll bonding (ARB) and high-pressure torsion (HPT), have been extensively researched to achieve the ultra-fine grain. HPT process can introduce the large amount of strain continuously compared to other SPD processes. Al-Li alloys has low density and are strengthened by dispersed fine precipitates through an aging treatment, traditionally. They have been used as aircraft materials. Yokota et al. reported the effect of Mg addition on Al-Li alloy, and Mg could promote the precipitation of the δ 'phase. This research investigated the effect of Mg addition on Al-Li alloys on grain refinement using HPT process and aging behavior. After HPT process, the grain sizes were refined about 200nm and Micro Vickers hardness increased significantly compared to as-quenched (asQ). During aging treatment, Al-Li-Mg alloy reached peak aging at 0.48 ks (8 min), however, Al-Li alloy did not change the hardness level at the initial stage of aging, then hardness started to decrease. Microstructure observation was carried out using as-HPT, 0.48ks, 3.84ks, and 600ks of aging time in both alloys. In asHPT sample, i.e. no aging treatment, δ’ phase was observed. With increase of aging time, it was possible to observe the coarsened δ’ phase.
Magnesium (Mg) has been widely used as structural materials, for example, frames for electrical devices, parts for automobiles, due to its light-weightiness. Several reports are available about addition of rare-earth elements (RE) on Mg. Mg alloys show precipitation hardening by aging treatment of super saturated solid solutions (S.S.S.S.). Lorimer el. al. reported the precipitation sequence in Mg-Y alloys aged at 473K as S.S.S.S. → β” (D019)→ β’(cbco) → β(Fm3 ̅m). Scandium (Sc) addition on Mg alloy is known that it enhances heat resistance. In this study, 3 kinds of Mg alloys (Mg-Y, Mg-Sc and Mg-Y-Sc alloys) containing the same total amount of solute elements, have been investigated to clarify the effect of the Sc on age-hardening and precipitation using HRTEM, SAED techniques and HRTEM simulations.
With increase of Y amount, Vickers microhardness increased during aging treatment. However, alloys with a large amount of Sc didn’t show age hardening. TEM observation was performed in under-aged, peak-aged and over-aged alloys. First-principles calculations were carried out using Bond Overlap Population (BOP) of DV-Xα.
In this paper corrosion properties and microstructure features of amorphous self-organised TiO2 nanotubes electrochemically deposited on titanium are discussed. There was titanium of second grade used as a substrate for these experiments. There was a specific solution of ammonium fluoride, ethylenglycol and deionized water used to create an oxide layer with advantageous properties. There were five anodized and one reference (non-treated) sample studied in this paper. Surfaces of the samples were mechanically prepared and surface roughness indexes was determined before and after anodization process. Relation between changes of roughness indexes before and after anodization was found out. The wettability (contact angle) of artificial plasma on surface was measured using sessile drop method. It was found out that titanium dioxide nanotubes formed on the surface significantly decreases contact angle and time of anodization reduces it even more. Corrosion potentials, corrosion rate or polarization resistance were determined by linear polarization methods performed by ASTM standards. Corrosion potential of anodized samples is substantially more positive (~ -50mV) compared with non-treated sample (~ - 280mV). On the other hand polarization resistance was significantly higher for non-treated sample. Also potentials of passive layer breakdowns were found. Non-treated sample showed remarkably higher breakdown potential (>7500 mV) than anodized samples (~3500 mV) for current density 10-4 A/cm2. There were electric capacity of oxide layer and its resistance defined by electrochemical impedance spectroscopy (EIS). Structure of nanotubes and influence of anodization on surface profile was studied by SEM. EDX was used for basic chemical analysis.
Nowadays, there is paying an attention using natural, renewable and biodegradable resource of raw materials, residues from agricultural processing as well cellulosic waste from agricultural crops or wood processing and papermaking industry and their utilization in building materials. The use of wood wastes in the production of wood-based materials has been considered environmentally sustainable, economically viable and socially acceptable. Also paper as well as recycled waste paper are considered as valuable material. The use of waste and natural cellulose fibres as reinforcement in cement composites has enormous potential in the field of recycled materials in building sector.
The objective of this study is to utilize cellulosic fibres coming from recycled waste paper into cement composites and characterise their impact on resulting physical and mechanical properties of fresh and hardened cement composites. Manufactured cement composites contained 0.2%, 0.3% and 0.5% addition of cellulosic fibres. Workability of fresh fibre cement composites was determined. Density as well as compressive and flexural strength of 28 and 90 days hardened fibre cement composites were tested. Distribution of cellulosic fibres with 0.5% addition in hardened fibre cement composites was also observed. The results showed reduction in densities of fibre cement composites with each fibres addition after 28 and 90 days of hardening what caused that these composites became lighter in weight. Mechanical properties of fibre cement composites have shown decreasing character with increasing amount addition up to 0.5% of cellulosic fibres into the mixture. Maximal decrease in compressive strength values were obtained in composites containing 0.5% of cellulosic fibres. However, obtained mechanical values of composites had satisfying results and also they are in conformity with European standard.
During austempering of higher-silicon steels, formation of bainitic ferrite is associated with carbon diffusion. Carbon diffusion is the cause of the increased carbon content in austenite in the vicinity of bainite sheaves. It occurs as a consequence of higher silicon levels, 1.5 to 2% weight percent, since silicon suppresses the naturally-occurring precipitation of carbides. The carbon content in the untransformed retained austenite is dictated predominantly by the austempering temperature and by the amount of newly-formed bainite. Therefore, the austempering conditions determine the ultimate stability of retained austenite upon final quenching to the room temperature. The present paper discusses the impact of the austempering temperature at a defined holding time on the amount of retained austenite in the microstructure of the unconventional 42SiCr steel with increased silicon level, and the effect of the amount of retained austenite on the ductile behaviour of steel.
Semi-solid processing is an unconventional technique which can be used to produce intricate components by forming. Besides that, the presence of molten phase leads to unconventional final microstructures. Using this route, one can for instance convert the sharp-edged carbides which are present in high-alloy tool steels. On the one hand, these carbides improve wear resistance of the material but on the other hand they also reduce its toughness, particularly when they are too large and their distribution is non-uniform. At high heating temperatures, they redissolve into the austenitic matrix and enrich it with alloying elements. However, the resulting microstructure at room temperature consists of polyhedral austenite grains and lamellar ledeburite network. The network can be removed from the microstructure by applying an appropriate deformation sequence during cooling.
X210Cr12 tool was experimentally processed by a combination of semi-solid processing and subsequent thermomechanical treatment in a hydraulic press. Because the heating temperature is an important parameter which dictates the liquid fraction in the microstructure, the experiment focused predominantly on testing its effect on microstructural evolution. The heating temperature was varied from 1200°C to 1280°C. It was found that an appropriate combination of heating temperature and hot plastic deformation leads to not only dissolution of primary chromium carbides but also their redistribution from the eutectic network to the matrix. By this route, very fine microstructures and hardness levels between 800 and 881 HV10 were obtained. The microstructures consisted of recrystallized grains of the M-A constituent and fine chromium precipitates.
Metakaolin based geopolymer binder was synthesized using variable factors such as Na2O/SiO2, Na2O/Al2O3 and H2O/Na2O molar ratios as well as curing time. Metakaolin was used as an alumino-silicate source incorporating with strong alkali activators; sodium hydroxide solution to undergo polycondensation and hence a formation of hardened geopolymeric binder. This work was aimed to investigate the effect of Na2O/SiO2, Na2O/Al2O3 and H2O/Na2O ratios, as well as curing time on phase transformation. The chemical composition, phase development and microstructure of reaction products were examined by X-ray fluorescence, X-ray diffraction analysis and scanning electron microscopy with respect to their final compressive strength. Increasing the molar ratios of Na2O/Al2O3 and H2O/Na2O tended to favour the transformation of amorphous gel to various types of crystalline zeolite. Sodalite (pseudo-phase zeolite) and zeolite belonging to the Faujasite group, as well as zeolite X and A were identified in these mixtures. Based on this study, systems that favoured the formation of zeolitic products tended to possess lower strengths.
In order to make better use of different active quicklime in the process of sinter granulation, the effect of quicklime activity on sinter granulation was studied. The results indicates that in the process of sinter granulation, the moisture content of different active quicklime is very different. Highly active quicklime requires more moisture in the process of sinter granulation, low active quicklime requires less moisture than highly active quicklime.Under the experimental conditions, the optimum moisture content of high activity quicklime is about 8.1, and the optimum moisture content of low active quicklime is about 7.3. For the quasi-particles, highly active quicklime has slightly better air permeability than low active quicklime at the optimum moisture content. For dry particles,-0.25mm the particle size of the low active quicklime was significantly more than the highly active quicklime.
The hypoeutectic Al-Si alloy using high pressure die-casting process is widely used for automobile parts because of excellent castability, mechanical properties and corrosion resistance. The microstructure of this alloy consists of the primary α-Al, eutectic Si phase and Mg₂Si phase. Mechanical properties depend on morphology of eutectic Si phase and Mg₂Si phase. In this study, Al-10%Si-Mg alloys perform gravity casting to the permanent mold with different diameter (φ15, 20, 35 and 65) cylinder-shape for changing cooling rate and investigated effect of magnesium content from 0% to 3.5% in solidification sequence. The cooling rate after crystallized primary aluminum phase were calculated in cooling curve, which increased with magnesium content in Al-10%Si alloy. In the hypoeutectic region and the hypereutectic region AlP acted as heterogeneous nucleation sites for eutectic Si phase and eutectic Mg₂Si phase, respectively.
The article evaluates the issue of work at heights in industry and reports statistics on fatal accidents at work, the source of which is a fall from above. It also deals with the assessment of the state of personal protective equipment already in use - for example, safety and working ropes and other accessories contaminated with facade paints, lyes, acids or mineral oils and their misuse and dangerous use. The state of the assessed personal protective equipment used was assessed in a test facility on test machines, where the safety of these devices was verified under certain conditions. The article also mentions the issue of inadequate training and training of high-level workers and the lack of training centers that carry out such training.
The present paper is focused on the workability of powder metallurgy workpiece (grade aluminium alloy EN AW 6082) prepared by equal channel angular rolling (ECAR) process, which belongs to the group of Severe Plastic Deformations (SPD) methods. The current research confirms that the main benefit of the process ECAR is the possibility to obtain much more continually-reproductive effective deformations in processed sample by a single pass in comparison to the other SPD technologies. The rigid-viscoplastic 3D finite element simulations (3D FEM) of the ECAR processes were performed and analysed using the commercial software DEFORM-3D. On the essential of the effective stress distribution, ECAR process can be divided into the four deformation zones: Shape Rolling - primary gripping zone, Upsetting – main gripping zone, SPD - shearing deformation zone and Extrusion zone - cross-sectional design. Each zone was described by dominated stress state in the workpiece and force distributions. Additionally, Cockcroft - Latham damage criteria were calculated regarding the workability assessment. Moreover, distribution of plastic deformation, strain rate and workability criterions were evaluated. The damage criteria were determined on the investigated material using the diametrical compression (DC) test. To verify the stress-strain conditions of the ECAR process resulting from the numerical simulations, one ECAR pass of the PM sample was performed on the real device.
Two high strength low alloyed steels with 0.4%C, 0.6%Mn, 2%Si and either 1.3%Cr or without Cr were used in this work to evaluate the effect of chromium on the final microstructure of high strength steel after thermo-mechanical processing. Various heating temperatures, cooling rates and bainitic hold temperatures were tested. High strengths around 1700 MPa were achieved for the chromium alloyed steel, however it was at the expense of low total elongation and chromium-free steel turned out to be better suited for TRIP (transformation induced plasticity) processing. The relatively high strengths around 900 MPa were in this case accompanied by very high total elongation exceeding 30%. The final microstructure of chromium free steel was also more typical for TRIP steel, as it consisted mainly of the mixture of bainite and polygonal ferrite.
Asymmetric rolling (ASR) as one of severe plastic deformation (SPD) methods, was used to create materials with ultra-fine grain structure leading to the improved performance of processing materials. This work show the evolutions of microstructure and mechanical properties during asymmetric rolling of pure aluminium. The asymmetric condition was presented by applying different roll diameters with ration of smaller and bigger roll 2,4. The thickness reduction of samples was at 20%, 40%, 70%, at ambient and cryogenic temperature. The experimental results show that asymmetrical rolling has a significant effect on deformation flow and can refine microstructure and improve the mechanical properties. Asymmetric rolling at cryogenic temperatures (ASR-C) allows to obtain greater strenght tensile properties about 10 MPa more as rolling at ambient temperatures (ASR-A) at equal observed conditions. Mechanical properties such as yield strength (YS) ultimate tensile strength (UTS) and micro-hardness were determined for all rolled samples.
Rare-earth orthoferrites RFeO3 (R =Rare earth) are a family of canted antiferromagnets showing a special variety of magnetic properties, such as complex spin reorientation (SR), novel multiferroics, magnetic refrigeration, and laser-induced ultrafast photomagnetic recording. The SR transition in rare-earth orthoferrites has gained wide attention because it is closely related to the ultrafast photomagnetic effect and the magnetic induced ferroelectricity. As we all konw that RFeO3 possesses two magnetic sublattices of Fe3+ (provide 3d-electrons) and R3+ (provide 4f-electrons) ions. People can find three types of magnetic interactions, Fe3+-Fe3+, Fe3+-R3+, and R3+-R3+ in these system. At Neel temperatures TN1 (~620–740 K, which is determined by Fe3+-Fe3+ interactions), a weak ferromagnetism (FM) originates from the slightly canted antiferromagnetism (AFM) in the Fe-sublattice. In addition, the R-sublattice only orders antiferromagnetically at lower Neel temperature TN2, which is determined by relatively R3+-R3+ interactions. In fact, these interesting magnetic behaviors are very sensitive to several external stimulations, such as applied magnetic field, temperature, and pressure etc.
According to some reports, PrFeO3 has a spin reorientation transition from Г4 (Gx, Ay, Fz) to Г2 (Fx, Cy, Gz) at 6-13K. SmFeO3 processes a transition from Г4 to Г2 state between TSR1=450 K and TSR2=480 K, which is the highest spin reorientation transition temperature of the whole RFeO3 family. It also has the compensation point Tcomp=4.9 K along a axis where the magnetization goes through zero and an obvious spin switching transition at TSSW=278.5 K (for H=300 Oe) in the M-T curve of SmFeO3.
In our work, we have grown 11 single crystal samples of Sm1−xPrxFeO3 (x = 0 to 1 with the interval of 0.1) by optical floating zone method. For x=0.5, the spin reorientation temperature is ~220 K, while the TSR= ~110 K for x=0.7. As for x=0.3, TSR is higher than room temperature. The result shows that with the increase of doping amount, the TSR decreases gradually. Moreover, for x=0.3, a spin switching is present, which is similar to that of SmFeO3. However, the doped samples are more sensitive to the low field in the normal temperature range.
Al-7mass%Si-0.3mass%Mg alloy is widely used for automotive components because it has excellent castability and higher strength and ductility by applying heat treatment. Age-hardening behavior of Al-7%Si-0.3%Mg alloy solution treated after cast into sand mold were investigated by Vickers hardness measurement, optical microscopic and scanning electron microscopic observation. This alloy is solution treated at 813K for 36ks and then artificially aged at 273-523K after water-quenched (W.Q.) and its aging behaviour was compared with that of Al-7%Si-0.3%Mg alloy that cast into permanent mold and heat treated at the same condition. Despite the fact that the alloy that cast into sand mold has a wider DASⅡ(secondary dendrite arm spacing) and the coarser crystallized phase than that of the alloy cast into permanent mold, age hardening behavior of the both alloys were almost the same.
It is known that mechanical properties of the Al-Mg-Si alloy can be improved by aging treatment due to formation and dispersion of fine precipitates, for example, G.P zones, β″(Mg5Si6), β′(Mg1.8Si) and β (Mg2Si). Cu and Ag addition on Al-Mg-Si alloy can enhance its mechanical properties because of solid solution hardening. Also, several reports about Cu and Ag addition on Al-Mg-Si alloy. In this research, (1) Al-1.0%Mg2Si [mol%] (base alloy), Cu and Ag add alloys have chemical compositions of (2) base-0.18Cu-0.18Ag [mol%](18CA alloy) and (3) base-0.35Cu-0.35Ag [mol%](35CA alloy) with fixed Cu/Ag ratio of 1.0 are prepared. Those alloys were fabricated by casting, then, alloys were subjected to homogenization treatment at 848K for 24 h. Solution treatment was carried out at 848K for 1 hr before aging treatment. Vickers microhardness measurement was conducted to estimate mechanical property after aging treatment. Microstructure observation was carried out using TEM. Ageing behavior carve by microhardness test shows 35CA alloy has best ageing hardenability than base alloy and 18CA alloy. TEM Observation form the [100]Al direction, It was possible to observe needle-like precipitations and their cross sectional planes. Needle-like precipitates have orientation relationship with matrix; parallel to the <001>Al direction.
Titanium dioxide coatings are widely used for technological applications due to their optical and photocatalysis properties. But, TiON coatings are usually fabricated by reactive sputtering using pure Ti target with O2 and N2 gas flow. We have developed new method for TiON coating by reactive sputtering method using TiO2 target with N2 and Ar gas flow. We previously reported that the X-ray diffraction patterns and TEM observation revealed that structure was changed from TiO2 rutile phase (nitrogen flow ratio:0%) to three kinds of mixed-phases of Ti3O5 monoclinic , TiO0.34N0.74 monoclinic and TiO2 rutile (nitrogen flow ratio:6%) by increasing of nitrogen flow ratio, N2/(N2+Ar). In this research, we prepared TiN / TiO2 bi-layer coating (nitrogen flow ratio:0%) and TiN / TiON bi-layer coating (nitrogen flow ratio:6%), and investigated the effect of the TiN under layer to the structure of the TiON layer. TEM observation revealed that TiN / TiO2 bi-layer coating showed the same phase as the TiO2 monolayer coating. On the other hand, TiN / TiON bi-layer coating showed the same phases but different plane orientations as the TiON monolayer coating. From this result, it is thinkable that there is no change in the phase to be generated, but the plane orientation of the TiON layer changed due to the effect of the TiN under layer.
The effect of welding parameters on lean duplex stainless steel welded joints by tungsten inert gas (TIG) process was studied. The weldments produced with different heat inputs were subject to microstructural, mechanical characterization using optical microscope, scanning electron microscope, Energy dispersive scanning and X-ray diffraction.
The HAZ in the lean duplex stainless steel is characterized by a high content of ferrite compared to base metal. This is due to the high peak of temperature induced during welding, where the structure is transformed to ferrite during thermal cycle of welding, and the austenite grains reformed by cooling to room temperature
The increase in hardness in the heat affected zone is due to the increase in the ferrite content in this zone
Potentiodynamic polarization tests of different welded joints show that weld metal structure composed of acicular secondary austenite is found to be more susceptible to pitting corrosion than those with primary one, which can be explained by the lower concentration of chromium, molybdenum and nitrogen in the secondary austenite than that in the primary austenite.
Two-step aging behavior of Al-7mass%Si-0.3mass% system alloy A356 cast into permanent mold and solution treated was investigated by micro-vickers hardness measurement, optical microscopy (OM) and transmission electron microscopy (TEM). The microstructure of as-cast state was consist of primary crystallized α-Al and secondary crystallized eutectic phases. The peak hardness increased almost the same value when the pre-aging temperature was 273K. On the other hands, positive effect of the final-aging was occurred after pre-aging at 348K and 423K with significantly increasing hardness in the under-aging region. Two-step aging behavior is considered due to the influence of precipitated phase mainly such as clusters and/or G.P.zone.
Plasma-chemical treatment (PCT) allows us to obtain completely new materials with widely varied surface properties, while preserving most properties of the original materials. This advantage is used in the activation of catalysts and adsorbents based on layered materials which represent an interesting opportunity for the development of new materials based on nano-design, controlled access to sites. PCT allows to modify surface area properties. The aim of this work was to study the influence of plasma-chemical treatment in O2 on the catalytic activity of copper-containing perovskites BICUVOX with the composition Bi4V2-2xCu2xO11–δ (х = 0.00–0.16) in isobutanol reactions.
Solid solutions were obtained solid-phase synthesis. All samples were studied in detail by means of DTA, XPA, and IR spectroscopy. In this work the catalytic characteristics of BICUVOX were obtained at temperatures up to 4000C in flow regime with chromatography analysis.
Plasma treatments lead to the total deactivation of the active sites of dehydration reaction, and the alcohol is converted with 100% selectivity into aldehyde. Activity of the dehydrogenation of alcohol after PCT increases in ~ 1.7 times on samples with xCu=0.04-0.06 compared to the initial samples. Similar values which were found for the samples with xCu=0.0-0.06, including the double vanadate, suggests that PCT affects the ceramic matrix with Bi, O and V elements. Addition of small amounts of copper does not change this effect.
Heusler alloys crystallize into a close-packed cubic structure, having a four-atom basis forming a face-centered cubic lattice. By selecting different composite elements, Heusler alloys provide a large family of members for frontier research of spintronics and magnetic materials, and devices. The structural, electronic and magnetic properties of a novel quaternary Heusler alloy, PdMnTiAl, have been investigated using a first principles computational materials calculation. We found that the stable ordered structure is a non-magnetic Y-type1, in good agreement with the Slater-Pauling rule. From the band structure and the density of states we predict that this Y-type1 configuration is a new gapless semimetal material. Furthermore, we discovered the Pd-Mn swap disordered structure to be more stable than the Y-type1 structure. Our present work provides a guide for experiments to synthesize and characterize this Heusler alloy compound.
Even after many years of routine treatment of conventional tool steels, novel and as yet unknown strategies and principles promising development of new processing technologies for these materials are still able to emerge. A high-alloy steel, such as X210Cr12 (1.2080) produced by conventional metallurgical routes, typically contains large sharp-edged M7C3 carbides which remain stable even at high temperatures. Consequently, these carbides are very difficult to alter and convert to other more beneficial configurations by heat treatment. This opens a possibility of using unconventional treatments to change the morphology of these carbides. One of the available techniques involves thermomechanical treatment in the semi-solid state. After semi-solid processing, the microstructure of X210Cr12 consists of polyhedral austenitic grains embedded in a ledeburite network where the latter comprises lamellar chromium carbides and austenite. The volume fraction of the network and the austenite grain size depend on the heating temperature. Several deformation steps applied at the experimentally-validated temperature of 1080°C, following heating in the range from 1200°C to 1280°C, can break up the ledeburite network. The deformation is applied in a hydraulic press. At an appropriate deformation magnitude and intensity, particles of the network can be redistributed within the austenitic matrix. This leads to a martensitic-austenitic microstructure with uniformly dispersed fine chromium carbides. The particle size in this carbide dispersion is approx. 400 nm, which contributes to the strengthening of the final microstructure and hardnesses around 850 HV10.
Thin films of Y-PSZ (yittria partially stabilized zirconia) were used as buffer layer in electro devices becouse of their chemical stability and insulation property. In this study, by applying the pulsed electric fields during the electrochemical deposition, the morphology control method of the depositted Y-PSZ films was investigated. Mixure of ZrO(NO3)4, Y(NO3)3 -6H2O were dissolved into water and then they were controlled nearly pH3 by adding NH3(aq) to make the precursor solution. The thin films were deposited on the glass substrate near the minus electrode by applying the electric field of 3.0 V for 20 min. In addition, another pulsed electric field of 0 to 10 Hz was applied to the perdicular direction to the film deposition direction. After annealing at 723 K for 6 h in air, the Y-PSZ films were crystallized. In the limited condition, the pinstripe patterns of YSZ films according to the frequency of the applied pulsed electrical field were observed. It was expected that ions movements in a precursor solution were restricted by the standing wave due to the applied pulsed electric field and therefore deposition area were limited. The cyclical correlation between the applied pulsed electrical field and the distances of pinstripes was also observed.
The purpose of this study was to develop a new low-temperature processing route for oxygen-free high thermal conductivity (OFHC) copper. This material exhibits high ductility and toughness even at low temperatures. Therefore, the main object of interest was the deformation behaviour and mechanical properties of pure copper at cryogenic temperatures. The processing route involved severe plastic deformation (SPD) applied in up to 6 passes through an equal channel angular pressing (ECAP) machine at room temperature. Products of various grain sizes were obtained and their microstructures and mechanical properties were examined and tested. Scanning electron microscopy with electron backscatter diffraction and transmission electron microscopy were used for microstructural characterization. Deformation behaviour was studied by tensile testing in a temperature interval between room temperature and 4.2 Kelvin. Various densities of deformation twins were found in the material, depending on the grain size and orientation after ECAP, and on the temperature of mechanical testing. In coarse-grain specimens, deformation took place not only by dislocation slip but also by twinning. After ECAP processing, copper shows relatively high yield strength across the entire temperature interval in question.
Friction stir welding (FSW) typically produces fine-grain structure in the welded region which is called “stir zone (SZ)”. The peculiar microstructure is responsible for improving mechanical properties of the joints, while thermal stability remains to be unsolved. The present paper describes abnormal grain growth which proceeds in the SZ during post weld heat treatment of 6061 aluminum alloy plate friction stir welded. The abnormal grain growth were typically observed to start in the region beneath the surface where the rotating shoulder touched followed by a preferential growth in the SZ until the entire region of SZ was occupied by these abnormally grew grains. This instability of microstructure is affected by some amount of residual strain caused by the shoulder passing by after the microstructure of SZ is produced by the rotating probe. A numerical simulation is also conducted to discuss the essential role of grain boundary migration in the peculiar microstructural evolution.
Thermoelectric materials based on Bi2Te3 exhibit a high performance at relatively low temperatures (below 400 K). Thus, these materials are used widely for the direct conversion of thermal energy into electrical energy and vice versa. The thermoelectric module used for this purpose is fabricated by electrically connecting several tens to hundreds of n-type and p-type thermoelectric elements in series onto a copper electrode prepared on a ceramic substrate, such as that of alumina (Al2O3). As these thermoelectric elements are connected in series, even a single defective joint can affect the thermoelectric conversion performance of the entire module. In the conventional thermoelectric module manufacturing method, a solder paste, which is a mixture of Sn alloy powder and flux, is applied on the copper electrode by screen printing method, and the thermoelectric elements are placed on top of it. Air heated to approximately 520 K is then used to melt the solder and bond the thermoelectric elements to the copper elec-trode. However, if the printing pressure during the screen printing process is not kept constant, the thickness of the solder paste layer becomes uneven, resulting in defective thermoelectric element bonding. To over-come this problem, a method for directly bonding thermoelectric elements onto the copper electrode without applying a solder paste was developed in this study. A coating of tin approximately 50 m in thickness was fabricated by electroplating on the surface of a Bi2Te3-based thermoelectric element, which had a nickel diffusion barrier layer. Subsequently, the tin-coated thermoelectric element was cut into pieces with dimensions of 3 mm 3 mm 3 mm using a wire saw, and the pieces were placed over a copper electrode. They were then subjected to direct thermocompression bonding at 523 K on a hotplate for 3 min under a pressure of 1.1 kPa. Scanning electron microscopy (SEM) imaging (Figure 1) confirmed that a strong and uniform bond was formed at the copper electrode/thermoelectric element interface, with the melted/solidified tin layer remaining defect free. Thus, the proposed method of fabricating thermoelectric modules by the direct thermocompression bonding of tin-coated thermoelectric elements with a copper electrode is a suitable way of ensuring a uni-form bonding interface without using solder paste.
Al-7mass%-Si-0.3mass%Mg system alloy is mainly applied to the automotive components, such as road wheel or suspension frame because of having higher strength, ductility and corrosion resistance. In this study, the age-hardening behavior and precipitation structures of Al-7mass%Si-0.3mass%Mg system alloys with T6 treatment were investigated by micro-vickers hardness measurement, optical microscopy and transmission electron microscopy. The alloy was cast into permanent mold, and then solution treated at 813K for 36ks and aged at 273K~523K. In the case of peak-aged at 523K in T6 condition, rod-shaped precipitates length of approximately 200nm were observed in the α-Al matrix. On the other hand, peak-aged at 423K in T6 condition, needle-shaped precipitates length of approximately 10nm were observed to be distributed high density in the α-Al matrix. These precipitates affected precipitated strengthening in the alloy.
Casting mold requires several performances, for example, high strength, good heat resistance, good toughness, good abrasion resistance, good thermal shock resistance, good machinability, good adhesion resistance. Steels are having sufficient strength as mold materials, however, they have an insufficient welding resistance, and can be improved by surface treatment. In this study, a different surface-treated molds; (1) nitride steel surface, (2) nitride steel surface coated with transition metal nitride thin film (hereinafter: nitride film) and (3) nitride steel surface coated amorphous carbon (a-C) film) were used. And, TEM samples were taken from the deposited Zn alloys on mold surface using FIB was observed, analyzed and compared by using TEM. From the cross-sectional TEM bright-field image of nitride steel having welded zinc alloy on mold surface, the thickness of welded zinc alloy was 4 ~ 5 μm. To investigate the interface phase between the zinc alloy and the nitride steel, the selected area electron diffraction (SAED) patterns were analyzed.
In the present work, WC-8(Ni,Fe) hard alloys were prepared from WC, Ni and Fe powders. The composition of metal binder was fixed at 8 wt.%, in which the amount of Fe was various from 1 to 4 wt.%. After ball milling for 72 h, the mixture powders were pressed and sintered by hot isostatic pressing (HIP) in Ar gas at the pressure of 7500 Psi and temperature of 1420oC. The results show a high potential of HIP process to obtain nearly full density of hard alloys, higher than 99 % of relative density of sintered alloys was reached in this work. The XRD analysis of sintered samples showed the main peaks of WC and a formation of NiFe phase rather than Ni and Fe individual phases. SEM images presented a homogeneity distribution of WC and metal binder. The measured Vickers hardness of hard alloys increased, as the content of Fe metal increased; meanwhile, fracture toughness has a tendency to decrease.
Identification of microstructure constituents is a prerequisite for studying the properties, technology and processing routes of steels. Conventional etching techniques may render identification of microstructures by means of optical microscopy difficult. This includes the cases when colour contrast between microstructure constituents upon etching is very weak or even absent. A typical example involves bainite and martensite which are virtually impossible to distinguish using ordinary techniques for revealing the microstructure by etching. Determination of phase fractions becomes very complicated and inaccurate when microstructure constituents are difficult to distinguish from each other. The present paper deals with the use of colour etching for identifying bainitic and martensitic microstructures in austempered steels and for developing sufficient colour contrast between microstructure constituents for quantitative assessment of phase fractions in intercritical-annealed steels.
Using first-principle calculations, we investigate two-dimensional (2D) honeycomb monolayer structures composed of group III-V binary elements. It is found that such compound like GaAs should have a buckled structure which is more stable than graphene-like flat structure. This results a polar system with out-of-plane dipoles arising from the non-planar structure. Here, we optimized GaAs monolayer structure, then calculated the electronic band structure and the change of buckling height under external electric field within density functional theory using generalized gradient approximation method. We found that the band gap would change proportionally with the electric field magnitude. When the spin-orbit coupling (SOC) is considered, we revealed fine spin-splitting at different points in the reciprocal space. Furthermore, the valence and conduction bands spin-splitting energies due to SOC at the K point of buckled GaAs monolayers are found to be weakly dependent on the electric field strength. Finally electric field effects on the spin texture and second harmonic generation are discussed. Another effective way to study the variation of electronic properties of GaAs monolayer is to apply the biaxial strain, both tensile and compressive, along the a and b axis. We can also obtained the transition from in-direct band gap to direct band gap. The present work sheds light on the control of physical properties of GaAs monolayer by the applied electric field and the biaxial strain.
Co4Nb2O9 and Mn4Nb2O9 was first prepared and studied by Bertaut et al.1 X-ray diffraction (XRD) studies showed that Co4Nb2O9 and Mn4Nb2O9 possess the same trigonal crystal structure (space group P3̄c1) with two formula units per cell. Magnetic structure has also been reported by Bertaut et al.1 and further confirmed by Schwarz et al.2 According to the results of neutron diffraction, below Néel temperature (about 30 K for Co4Nb2O9 and 125 K for Mn4Nb2O9), both Co and Mn ions spin order along the c axis and form chains along the lines (1/3,2/3,z) (+spins) and (2/3,1/3,z) (-spins) with antiparallel inter-chain coupling. N.D.khanh et al.3 investigated single crystals of the Co4Nb2O9 by neutron diffraction and magnetic susceptibility measurement. The results suggest that Co2+ magnetic moments are mainly in the ab plane with small canted moments along c axis, which is different from previous report. In contrast to Co4Nb2O9, the antiferromagnetic transition order of Mn4Nb2O9 single crystal is along c axis by Yiming et al. 4
In order to control the direction of magnetic moments, we doped the Mn ions in Co4Nb2O9. In this work, single crystals of Co2Mn2Nb2O9 and CoMn3Nb2O9 were successfully grown by optical floating zone method. X-ray diffraction (XRD) indicates that it has a single phase corundum–type structure. M-T curves shows that the direction of magnetic moments for Co2Mn2Nb2O9 and CoMn3Nb2O9 are both similar to that of Co4Nb2O9. This phenomenon indicates that strong coupling between and Co2+ and Mn2+. Furthermore, the strong coupling between Co2+ and Mn2+ could be modulated by the external magnetic field and temperature. REFERENCES: 1. E. F. Bertaut, L. Corliss, F. Forrat, R. Aleonard and R. Pauthenet, Journal of Physics and Chemistry of Solids 21 (3), 234-251 (1961); 2.B. Schwarz, D. Kraft, R. Theissmann and H. Ehrenberg, Journal of Magnetism and Magnetic Materials 322 (5), L1-L3 (2010); 3.N. D. Khanh, N. Abe, H. Sagayama, A. Nakao, T. Hanashima, R. Kiyanagi, Y. Tokunaga and T. Arima, Physical Review B 93 (7), 075117 (2016); 4.Y. Cao, M. Xiang, Z. Feng, B. Kang, J. Zhang, N. Guiblin, W. Ren, B. Dkhil and S. Cao, RSC Advances 7 (23), 13846-13850 (2017).
RFeO3 (where R is a rare-earth ion) perovskite oxides with canted antiferromagnetism has attracted the attention of researchers to explore interactions involving two spin sublattices. The potential applications in technologies of RFeO3, such as complex spin reorientation (SR), magnetic refrigeration, and novel multiferroics, has been extensively studied. The reason for the diversity of magnetic properties characterized of RFeO3 is usually due to two kinds of magnetic sublattices of Fe3+ and R3+ ions. At Neel temperatures (TN1=620–740 K), the Fe3+-Fe3+ interactions cause an ordering of the Fe3+ ions, while the R3+ ions order magnetically below a separate, lower Neel temperature TN2 ,which is determined by relatively R3+–R3+ interactions. Above TN2, the R3+ ions are partially magnetized by the molecular field of the ordered Fe3+ ions. In general, three types of magnetic interactions that exist in the RFeO3, Fe3+-Fe3+, Fe3+-R3+, and R3+-R3+ respectively.
Many RFeO3 crystals exhibit characteristic spin-reorientation (SR) transition, in which the direction of the net moment changes from one crystal axis to another or be antiferromagnetism. According to some reports1, ErFeO3 processes a spin reorientation transition from Г4 (Gx, Ay, Fz) to Г2 (Fx, Cy, Gz) state at a temperature range of 88K≤TSR ≤97K, and have the compensation point Tcomp =46 K along a-axis where the magnetization goes through zero. In addition, anomalous jump also exist in the M-T curve of ErFeO3. Many RFeO3 crystals exhibit characteristic spin-reorientation (SR) transition induced by temperature and/or an applied magnetic field. Because of the absence of f electron in Y3+ ions, temperature induced SR transition cannot appear in YFeO3, however, magnetic field induced SR in YFeO3 has been studied in THz time-domain spectroscopy experiment2. The reorientation temperature of the orthoferrites also can be altered by compositional variation. Dropping behavior would expect an approximately linear decrease in the spin reorientation temperature.
In this work, we have grown 5 single crystal samples of Er1−xYxFeO3 (x=0, 0.25, 0.5, 0.75, 1) by optical floating zone method. A temperature-induced SR transition between Г4 and Г2 was observed by subsequent magnetic measurements. The M-T curves show that, along with the increase of Y3+ component in Er1−xYxFeO3, we observed a decrease in the spin reorientation temperature. When x increases to 1, there is no SR transition in YFeO3. In addition, the typical compensation point of ErFeO3 also decreases with dropping behavior, Er0.75Y0.25FeO3 has the compensation point Tcomp =38 K along a-axis and Er0.25Y0.75FeO3 almost exhibit no compensation point.